View Single Post
  #4 (permalink)  
Old 04-09-2009, 05:10 AM
KHK's Avatar
KHK KHK is offline
Moderator
 


Join Date: Oct 2008
Location: Chicago suburbs
Posts: 961
Thanks: 2
Thanked 1 Time in 1 Post
Groans: 0
Groaned at 0 Times in 0 Posts
Rep Power: 37
KHK is on a distinguished road
The only problem I have had is with powder coated metal. It does not seam to work to well.

keith
__________________
keith

The older the Boys, the more expensive the TOYS
Previously Owned equipment;
Miller gas welder, Union Carbide 400 amp ac/dc/tig welder, Dayton 230 amp ac/dc welder with Miller 400 amp HF unit.
LS-160P
Current equipment;
3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch,
2 Longevity autodarking helmets
WeldAll 200PI