First welds with the Weldall 200PI Be gentle!
Here are some welds with my 200PI. I'm rustier that the mower blades I'm practicing on. I was using 3/16" 6013 rods. The pass down the middle is at 70 amps AC. The upper right was also 70 amps and it has some under cutting. The one on the left is 60 amp AC. less under cut.
Any suggestions would be appreciated.
I know I need more practice and a welding table. This welding on the floor is a pain in the knees.
Weldall 200PI, Longevity Pro auto-darkening hemet, HF 120amp stick welder (retired), Quincy 60 gallon 5hp air compressor, Iron Mike power hack saw, HF 42144 3-in-1 , 20 ton press, and a screw driver but I'm not sure where I left it...