and i found the one i wanted only to find its been discontinued (200p)
so i called longevity and they suggested the 200d ? not as portable but its what they offer
when i got it the owners manual didnt say anything about it being multi voltage or how to wire it correctly
it claims 220/240 vac is acceptable but it comes with a 110 vac plug that i've never seen before so i had questions and calledleft 2 messages and haven't heard back
i like the machine and have it in use and it works great. just wish the literature was more in depth and left me with fewer questions
it seems to work fine with regular 110v ac 20a circuit and it automatically reduces the output to 95a but thats plenty for 3/32 rodor even 6010 1/8 so thumbs up on this one