How well does a plasma cutter work on kitchen metal? I remember trying to drill the stuff a while ago and it's was crazy hard!!!
How well does a plasma cutter work on kitchen metal? I remember trying to drill the stuff a while ago and it's was crazy hard!!!
It will cut it just fine.
He's probably talking about stainless thats my guess anyway.
Kitchen metal? What is that.
More like stainless , yes it will work with plasma.
Plasma cutters work great on stainless!!
keith
The older the Boys, the more expensive the TOYS
Previously Owned equipment;
lot's
Current equipment;
3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
2 Longevity autodarking helmets
160d MIG
WeldAll 200PI
Most likely i am talking about stainless in the construction field they install this metal in commercial kitchen and referr to the metal as kitchen metal so idk but that would make sense we will stick to stainless was just wondering if some metals are harder to cut then others???
It’s probably 316 stainless steel in a commercial kitchen, I have used my plasma cutter to cut 316 and 304 stainless and it cuts it like a hot knife through butter.
well thats a plus if i ever get in a jam again with that stuff ugh