Here is a typical cut on .07 Stainless Steel
Settings;
Air pressure.. 60 PSI
Amps.. 40
The left side of the last picture is showing the cut free-hand. WOW I gues tha I am shaker than I thought!!
The right side is using a tip spacer and a guide.
Here is a typical cut on .07 Stainless Steel
Settings;
Air pressure.. 60 PSI
Amps.. 40
The left side of the last picture is showing the cut free-hand. WOW I gues tha I am shaker than I thought!!
The right side is using a tip spacer and a guide.
keith
The older the Boys, the more expensive the TOYS
Previously Owned equipment;
lot's
Current equipment;
3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
2 Longevity autodarking helmets
160d MIG
WeldAll 200PI
Nah.
You are an "Interpretive Metal Performer"![]()
Uncle Ed
Longevity Weld-All LS-200PI (TIG/ARC/PLASMA)
Lincoln Weld Pak 3200HD (MIG)
UniWeld Handy Tote O/A Torches (Fire Maker)
Northern Tool ADF750S ADF Helmet (I like lots)
Chicago (HF) Eagle ADF Helmet (Like not so much)
Speedway ADF Helmet (Emergency Spare)
Shurefire Propane/Map Torches
| www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map |
Bookmarks