Had a drop blow through my plasma hose.....Where can I get a replacement?
Cheaply.....
Had a drop blow through my plasma hose.....Where can I get a replacement?
Cheaply.....
So I found some trafimet clones on ebay but have to wait a month to get them, and I dont really need the whole assembly, just the actual hose. Any ideas, going to the LWS tomorrow to see what they say about a replacement for the hose.
This is not making me feel warm and cozy about this machine.....
You mean you had a blowout in the torch hose? If so what air pressure were you set at or was it from plasma splatter? Contact Jesse and see what he can do for you. Phone will be quicker for you.
Units owned
Longevity WeldPro LS200PI (IGBT)
Force Cut LP80 plasma cutter
Longevity auto dark welding helmet
Atlas 10x36" lathe
Craftsman 5HP 30 Gal compressor
Home made CNC router/plasma cutting table powered by Longevity Force Cut LP80
Home built aluminum foundry, HF 4x6 bandsaw, O/A torch
No a drop from cutting melted the hose
I see they make leather sheaths to cover an entire plasma hose. Guess I know why now!
Longevity LP-60I Plasma Cutter
Hobart Handler 150
Weld Mark 295A Infinite Buzzbox
Arcair Carbon Arc Cutter
| www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map |
Bookmarks