does the tip touch the surface you are cutting....or do I need to switch to decaf?
does the tip touch the surface you are cutting....or do I need to switch to decaf?
You should try to keep the tip 1/16 to 1/8 above the material being cut.
Longevity ForceCut 40I Plasma Cutter
Longevity Elite Carbon Fiber Helmet
Lincoln Power MIG 180C
Miller Spectrum 375 Plasma Cutter
HF Mig100
HF 80 Amp Inverter Arc Welder
Bar and Rod Bender w/ scroll attachment
Various grinders, clamps, and stuff
old97 (03-24-2011)
This depends on the type/age of the cutter. The older cutters were drag cutters and you had to drag the tip to make a cut. All of current Longevity cutters do not need to to touch the metal to cut. The consumables will last much longer with a non contact. Longevity sells two types of spacers to help maintain cutting distance. The roller type cost about $40 and the spring type cost about $12
Last edited by KHK; 03-25-2011 at 01:39 AM.
keith
The older the Boys, the more expensive the TOYS
Previously Owned equipment;
lot's
Current equipment;
3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
2 Longevity autodarking helmets
160d MIG
WeldAll 200PI
When I free hand a cut I seem to bounce off the surface a lot. I try to keep a slight angle so that the flame will not bounce straight back up the nozzle greatly reducing the life of the tip. I too feel like I have caffeine jitters so I go to great lengths to make holders to guide the torch. I have never tried the two wheel holder, but feel it would work well. I think a simple ceramic cup with a hole in it could be strapped to the tip for controlled dragging, but would block ones view.
"Man is the best computer we can put aboard a spacecraft ... and the only one that can be mass-produced with unskilled labor"
Apollo 11 W.V. Braun
Have ForceCut80I, Precision TIG 185, Ideal Arc 250, Oxy-Acetylene, Tig welding Chamber, 14 Ton pipe bender, 20 Ton press, Electric sheet metal shear, 12 inch- 0.125 Shear, 12 inch Metal Band Saw, Power Hack Saw, Abrasive Chop Saws, 2 Mills, 5 Lathes, and lots of other items
I have a 40D and when I bought mine I wanted to buy the roller spacer but was told it would not fit the 40D so I got the spring spacer and it works fine . I think $12 dollars is a little high for the little spring wire
I put my left hand under the torch and use it as a steady prop to keep it balanced, steady, and a consistent height while using my right hand to actually operate the torch. It helps if you try to keep everything as steady and consitent as possible because the more jerky and unstable you are, the more clean up you will have to do to smooth everything out.
Just Sensible Concepts
*Longevity Weldall 160PI (technically it's not mine but it is on MY inventory for my shop at work)
Lincoln Weldanpower 200
Lincoln Pro Mig 180
Lincoln AC225
Hello Bluesman,
Full pilot arc plasma cutting torchs are not meant to have the tip touch the metal as plasma cutters without pilot arc do, have a great day.
Best,
DP
Last edited by LONGEVITY-Support; 11-08-2011 at 11:19 AM.
Sincerely,
LONGEVITY Customer Service
Toll Free: 877-566-4462
Email: help@longevity-inc.com
Website: www.longevity-inc.com / www.lweld.com
Racing Site: www.longevity-racing.com
X2 on what Bluesman said. I rest my torch on the non pulling hand as well. I find it steadies me as well as keeping the tip a safe distance away from the work.
HTP Mig 2400
HTP Microcut 625
Longevity Tigweld200
Hubangus blast cabinet
Enco Mill
O/A torch setup
PT105 Bender
Notchmaster
4X6 bandsaw
Portaband
20T press
| www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map |
Bookmarks