Anyone know of a cutting chart for the 50i plasma cutter...
deplicting cut speed, metal thickness, amps needed...
I'd like to have it for reference with my CNC table...
im going to be cutting 1/2" mild...
thanks
Anyone know of a cutting chart for the 50i plasma cutter...
deplicting cut speed, metal thickness, amps needed...
I'd like to have it for reference with my CNC table...
im going to be cutting 1/2" mild...
thanks
Longevity Arcmate 160
Longevity 50i
Longevity TigWeld 200 DX
Longevity Water Cooler
Torchmate 2x2
Custom Water Table
HF 4X6 Bandsaw
Custom Built 16" Chop saw
Grizzly 14" band saw
Delta 6" vert. belt sander
Victor O/A
Craftsman 5hp, 30gal
Delta Drill Press
I cut some 1/2-9/16 angle iron with my CNC and used the following settings.
Air pressure 55 psi
Amps - 50
Travel 6 IPM (lots of slag, but removal was easy )
8 IPM (much less slag, harder to remove.)
Machine - 200pi
keith
The older the Boys, the more expensive the TOYS
Previously Owned equipment;
lot's
Current equipment;
3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
2 Longevity autodarking helmets
160d MIG
WeldAll 200PI
| www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map |
Bookmarks