Afrikaans Arabic Belarusian Bulgarian Catalan Czechoslovakia Cyprus Germany  Spanish  Ethiopia Persian Finnish French Irish Galician Hindi Croatian Hungarian Icelandic Italian Hebrew Japanese Korean Italian Latvian, Lettish Macedonian Malay Maltese Dutch Norwegian Polish Portuguese Romanian Russian Slovak Slovenian Albanian Serbian Swedish Swahili Thai Tagalog Turkish Ukrainian Vietnamese English
FreeWeldingForum.com Welding Forum Community presented by LONGEVITY  
+ Reply to Thread Share
Results 1 to 4 of 4

Thread: TIG WELD 200 Review

  1. #1
    steveo928 is offline Member
    Join Date
    Mar 2010
    Posts
    33
    Images
    1
    Thanks
    4
    Thanked 11 Times in 5 Posts

    TIG WELD 200 Review

    I recently received A TIG WELD 200 from longevity to review and I love it. The pulsing is an incredible feature that is very useful in some applications near edges.
    The 200 AMP TIG output is more than enough for the things I do, and it can easily penetrate 1/4" mild steel. The Stick welding on the machine is very smooth and can weld some pretty hefty material. With 160 amps of power, 5/32 electrodes can be used.
    I love the machine, and would recommend to anyone.

    -steve


  2. The Following 2 Users Say Thank You to steveo928 For This Useful Post:

    Gadget (01-15-2011), poodle (01-16-2011)

  3. #2
    poodle's Avatar
    poodle is offline Senior Member
    Join Date
    Jul 2010
    Location
    Texas
    Posts
    319
    Images
    21
    Thanks
    5
    Thanked 15 Times in 15 Posts
    Hey Steve, I really enjoyed your video. I could hear how smooth the machine was on it. Even when you switched over to stick it still sounded nice and smooth. I was holding out for a multi-purpose mach. but I really just want a TIG so you may have just sold me on this one. One little bit of advice, Put on some safety glasses. That little peck with the hammer or a flick of that brush could mean a trip to the doc's. Just from someone who has been there. Loved the video, thanks.
    Steve
    Miller Dialarc 250
    Lincoln Ranger250
    Longevity TigWeld 200DX

  4. #3
    tomsign Guest
    Steve, nice video and review, I also 2nd Poodle on the safety glasses (been there)
    Tomsign

  5. #4
    steveo928 is offline Member
    Join Date
    Mar 2010
    Posts
    33
    Images
    1
    Thanks
    4
    Thanked 11 Times in 5 Posts
    I really would bet this machine If I was you!! Its small, lightweight, and perfect for some pretty hefty fab.
    And just cause of you guys, I will wear safety glasses from now on, and trust me, I know what you mean cause I've gotten hot slag in my eye.. Not fun at all.

+ Reply to Thread Share

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
 
 
www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map