Automatic Translations (Powered by Powered by Google):
Afrikaans Arabic Belarusian Bulgarian Catalan Czechoslovakia Cyprus Germany  Spanish  Ethiopia Persian Finnish French Irish Galician Hindi Croatian Hungarian Icelandic Italian Hebrew Japanese Korean Italian Latvian, Lettish Macedonian Malay Maltese Dutch Norwegian Polish Portuguese Romanian Russian Slovak Slovenian Albanian Serbian Swedish Swahili Thai Tagalog Turkish Ukrainian Vietnamese English
FreeWeldingForum.com Welding Forum Community presented by LONGEVITY  
+ Reply to Thread Share
Page 2 of 2 FirstFirst 12
Results 11 to 12 of 12

Thread: Internal Gas Solenoid Info?

  1. #11
    KHK's Avatar
    KHK
    KHK is offline Moderator
    Join Date
    Oct 2008
    Location
    Chicago suburbs
    Posts
    2,565
    Images
    88
    Thanks
    0
    Thanked 52 Times in 50 Posts
    What are the specks on the filter? Max PSI? Volume?
    keith
    The older the Boys, the more expensive the TOYS
    Previously Owned equipment;
    lot's
    Current equipment;
    3HP Speedair air compressor, Wilton drill press, Craftsman 10x36 lathe, 10 ton hydrolic press, Portaband band saw, OA torch, Small home brew CNC machine, powered by my 200PI
    2 Longevity autodarking helmets
    160d MIG
    WeldAll 200PI

  2. #12
    WookieWelding's Avatar
    WookieWelding is offline Senior Member
    Join Date
    Jan 2011
    Location
    Socal
    Posts
    554
    Images
    61
    Thanks
    2
    Thanked 19 Times in 17 Posts
    Quote Originally Posted by tigqk View Post
    I know their have been some welders that did not like the idea of the argon and air line using the same lines. I have heard warnings about using rubber on tigs, but no reason to suspect mine has any water in the lines.If anyone likes to add another filter you could try this as your final air separator for your system, before it enters the machine, it is also small enough that you could run it on the inside quite easy.I think their is a treated paper medium on the inside, and these filters are meant to be disposable, they are about $5.00-$7.00.
    sorry for Hijack there is no issue with rubber power cables or gas hoses here is a lil info YouTube - TIG Cable and Hose Materials--What's the Difference?
    TigWeld 250
    old 1950s Master Electric engine drive DC Powersource
    HF 151 Mig
    HF 100 FC
    Victor Journeyman Oxy/Ace set up
    Bunch of tools of the trade to much to list
    WeldorWeb.com

  3. The Following User Says Thank You to WookieWelding For This Useful Post:

    arandall (04-10-2011)

+ Reply to Thread Share
Page 2 of 2 FirstFirst 12

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
 
 
www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map