Afrikaans Arabic Belarusian Bulgarian Catalan Czechoslovakia Cyprus Germany  Spanish  Ethiopia Persian Finnish French Irish Galician Hindi Croatian Hungarian Icelandic Italian Hebrew Japanese Korean Italian Latvian, Lettish Macedonian Malay Maltese Dutch Norwegian Polish Portuguese Romanian Russian Slovak Slovenian Albanian Serbian Swedish Swahili Thai Tagalog Turkish Ukrainian Vietnamese English
FreeWeldingForum.com Welding Forum Community presented by LONGEVITY  
+ Reply to Thread Share
Results 1 to 6 of 6

Thread: railing complete with "baskets" (bluesman)

  1. #1
    SICFabrications's Avatar
    SICFabrications is offline Senior Member
    Join Date
    Jul 2010
    Location
    central arkansas
    Posts
    1,046
    Images
    43
    Thanks
    33
    Thanked 99 Times in 85 Posts

    Awards Showcase

    railing complete with "baskets" (bluesman)

    this railing has them baskets in it, bluesman
    Attached Images Attached Images   
    Torchmate 5 x 10 custom built CNC table
    6 (each) Thermadyne 252i mig/ stick/ tig
    Thermal Dynamics a-60 automated cutter
    Thermal cutmaster 52 handheld cutter
    '07 pro300 miller
    '08 275 trailblazer miller
    '99 250 trailblazer
    12vs extreme suitcase feeder
    2 (each) xr-a 50 foot push-pull feeders (for aluminum mig)
    800 ton break
    400 ton shear
    MM350p
    xmt 304
    (do i REALLY need to keep going?)

    nothing fancy, just a few hot glue guns for metal

    www.sicfabrications.com

  2. #2
    Bluesman's Avatar
    Bluesman is offline Senior Member
    Join Date
    Feb 2010
    Location
    South MS
    Posts
    712
    Images
    51
    Thanks
    200
    Thanked 18 Times in 18 Posts
    Very nice! I may have just told Sanderson Farms to kiss my arse so maybe not in chicken business for very long therefore I may in the near future be able to take a "vacation" up to Arkansas to visit with you perhaps, once I get un-broke that is.
    Just Sensible Concepts
    *Longevity Weldall 160PI (technically it's not mine but it is on MY inventory for my shop at work)
    Lincoln Weldanpower 200
    Lincoln Pro Mig 180
    Lincoln AC225

  3. #3
    SICFabrications's Avatar
    SICFabrications is offline Senior Member
    Join Date
    Jul 2010
    Location
    central arkansas
    Posts
    1,046
    Images
    43
    Thanks
    33
    Thanked 99 Times in 85 Posts

    Awards Showcase

    come on then.... i would even put ya up at my place (for a lil bit anyway, ya might smell funny)
    Torchmate 5 x 10 custom built CNC table
    6 (each) Thermadyne 252i mig/ stick/ tig
    Thermal Dynamics a-60 automated cutter
    Thermal cutmaster 52 handheld cutter
    '07 pro300 miller
    '08 275 trailblazer miller
    '99 250 trailblazer
    12vs extreme suitcase feeder
    2 (each) xr-a 50 foot push-pull feeders (for aluminum mig)
    800 ton break
    400 ton shear
    MM350p
    xmt 304
    (do i REALLY need to keep going?)

    nothing fancy, just a few hot glue guns for metal

    www.sicfabrications.com

  4. The Following User Says Thank You to SICFabrications For This Useful Post:

    Bluesman (02-03-2012)

  5. #4
    Nick's Avatar
    Nick is offline Senior Member
    Join Date
    Feb 2011
    Posts
    525
    Images
    11
    Thanks
    2
    Thanked 13 Times in 13 Posts
    Sic,

    Wondering if you bent the baskets on site. Seems like something most wouldn't, but we know your affinity for custom bending and twisting jigs.

    I've seen it done w/ a forge and twisting rig before. Very cool either way though.
    Full hand tool assortment, collecting sheet metal hammers/dollies, more time than money.

  6. #5
    exwldr's Avatar
    exwldr is offline Junior Member
    Join Date
    Jan 2012
    Location
    Pennsylvania
    Posts
    21
    Images
    20
    Thanks
    0
    Thanked 2 Times in 2 Posts
    very nice railing, the baskets are awesome!

  7. The Following User Says Thank You to exwldr For This Useful Post:

    SICFabrications (02-01-2012)

  8. #6
    tomsign Guest
    Stan,
    nice as all ways

  9. The Following User Says Thank You to tomsign For This Useful Post:

    SICFabrications (02-01-2012)

+ Reply to Thread Share

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
 
 
www.longevity-inc.com | About us | Products | Rentals | Resources | Dealers | Order Status | Contact us | Help & Faqs | Site Map