- Features
- Specifications
- Similar Models
- What's Included
- Recommended Accessories
- Article & Resources
- Warranty
- Videos
- Reviews
- Q & A
|
Input |
110v 50/60hz 1 phase |
|
Spool Gun Capable |
YES with Optional SpoolGun140 |
|
Technology |
Inverter Based |
|
Duty Cycle |
20% @ 90A 18V |
|
Stick Welding Capable |
NO |
|
Wire Range |
.025”-.030” (0.6-0.8mm) solid steel |
|
Dimensions |
W: 9.6” x H: 14.5 ” x D:16 ” |
|
Weight |
40 lbs |
| Product Literature : |
|
|||
| Warranty : |
|
|||
|
|
MIGWELD 100 |
MIGWELD® 140 |
ARCMATE® 205p |
MIGWELD® 200 S |
|
|
| Rated Input |
120VAC, 60 Hz, 18 Amps | 115VAC, 60 hertz, 20 amps | 1 Phase220-240VAC 50/60hz | 1 Phase220v 50/60hz | 1 Phase or 3 Phase 220v 50/60hz | 3 Phase 220v 50/60hz |
| Technology | INVERTER | Infineon IGBT | Infineon IGBT | INVERTER | Infineon IGBT | Infineon IGBT |
| No Load Voltage | 31v | -- | 55-75v | 50-80v | 55-75v | 55-75v |
| Rated Input Current | -- | -- | 34 A |
37.4A | 1 Phase: 40Amps 3 Phase: 23Amps | 3 Phase: 37 A |
| Rated Input Power |
-- | -- | 7.5Kva | 7.5Kva | 9 Kva |
9 Kva |
| Power Factor | -- | -- | 0.8 | 0.73 | .08 | .08 |
| Efficiency | -- | 85% | 0.80 | 85% |
85% | |
| Voltage Adjusting Range | -- | -- | 14-26v | 15.5-24v | 14-28v | 16-28v |
| Current Output Range | 50-100 Amps | 20-140A | 40-200A | 30-200A | 40-250A | 40-300A |
| MIG Min./Max. Output (Amps) |
10%@100amps | 30-140Amps: 20% Duty Cycle at 140 Amps |
200amp duty cycle is 40% 155amp duty cycle is 60% 120amp duty cycle is 100% | 200amp duty cycle is 60% | 250amp duty cycle is 35% 200amp duty cycle is 60% 160amp duty cycle is 100% |
40-300Amps 35% Duty Cycle at 300 Amps |
| Wire Speed | -- | 59 to 393 in/min (1.5-10.0m/min) |
59 to 393 in/min (1.5-10.0m/min) | 59 to 393 in/min (1.5-10.0m/min) | 59 to 393 in/min (1.5-10.0m/min) | 59 to 393 in/min (1.5-10.0m/min) |
| Maximum Spool Size Capacity | -- | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder |
| Suitable Wire | Welding wire size:.035" to 040" | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. |
| Spool Gun Capable | NO | SPOOL GUN 140 | Speed Adjust 8M Spool Gun | SPOOL GUN 140 | Speed Adjust 8M Spool Gun | Speed Adjust 8M Spool Gun |
| Weld Aluminum | NO | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN |
YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN |
| GMAW-P (Pulse MIG feature ) | NO | No | Yes | No | Yes | Yes |
| Stick Welder (Option) | NO | -- | 40-160Amps 60% Duty Cycle at 160Amps | 30-200Amps 60% Duty Cycle at 160Amps | N/A | N/A |
| DC Stick Material Thickness | -- | -- |
.012- 1/2" | .012- 1/2" | -- | -- |
| Stick ( ARC ) Electrode Maximum Diameter (E7018) | -- | -- | 5/32" | 1/8" | 3/16" | 1/4" |
| Weldable Materials |
Mild Steel | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun |
30-140Amps:
20% Duty Cycle at 140 Amps
20% Duty Cycle at 140 Amps

LONGEVITY 140 AMP MIG WELDER SPOOL GUN CAPABLE 110V.
• MIG Torch with contact tips (3 meters)
• Earth/Ground Clamp (3 meters)
• Regulator Flow Gauge
• .030 and .035 contact tips
Accessories for this item
Related Articles
Related Videos
Product Literature
Additional resources
Welding Resources
- Excellent welder Review by Fergal
-
With this welder I can do accurate welds with no slag and little fumes. Now I can weld aluminum without any problem using spool gun. No complaints about customer service. Delivery was made without delay. (Posted on Apr 27,2013)
- Exceptional Mig welder Review by Jeff
-
It is really an exceptional machine for the price. I acquired this welder to weld aluminum in a garage. It provides high welding speed and control on material. Now, I can get clean and accurate welds with little slag. It is setup easily. In addition, I got a lot of included extras.
(Posted on Apr 25,2013)
- I recommend you to acquire this welder Review by Edgar
-
I have bought this welder to use in workshop for welding parts of trawl doors. I am completely satisfied with welding productivity and materials consumption rate. Thermal overload protection extends the lifetime of the device. It is easy operated; its portability is very suitable for my job because I have to move around a lot. Besides, when buying a welder I was surprised to get included extras-welding wire roll, welding mask, hammer, welding brush,and gas regulator (Posted on Apr 23,2013)
- test Review by carlos
-
test (Posted on Apr 23,2013)
- all-purpose welder Review by Ricardo Montoya
-
Good welder!!! Industrial quality steal for 3 hundred bucks. Works for aluminium with additional spool gun which you may want to buy separately on the same site, not included Creates nice looking accurate welds with a little practice. Easy to operate. Very satisfied, thank you. (Posted on Apr 13,2013)