Input |
220v 50/60hz 1 phase |
|
Spool Gun Capable |
YES with Optional SpoolGun140 |
|
Technology |
Transformer |
|
Duty Cycle |
60% @ 200A |
|
Stick Welding Capable |
YES |
|
Wire Range |
.025”-.030” (0.6-0.8mm) solid steel |
|
Dimensions |
W: 10.75” x H: 17 ” x D:20 ” |
|
Weight |
37 lbs |
| Product Literature : |
|
|||
| Warranty : |
|
|||
|
|
MIGWELD 100 |
MIGWELD® 140 |
ARCMATE® 205p |
MIGWELD® 200 S |
|
|
| Rated Input |
120VAC, 60 Hz, 18 Amps | 115VAC, 60 hertz, 20 amps | 1 Phase220-240VAC 50/60hz | 1 Phase220v 50/60hz | 1 Phase or 3 Phase 220v 50/60hz | 3 Phase 220v 50/60hz |
| Technology | INVERTER | Infineon IGBT | Infineon IGBT | INVERTER | Infineon IGBT | Infineon IGBT |
| No Load Voltage | 31v | -- | 55-75v | 50-80v | 55-75v | 55-75v |
| Rated Input Current | -- | -- | 34 A |
37.4A | 1 Phase: 40Amps 3 Phase: 23Amps | 3 Phase: 37 A |
| Rated Input Power |
-- | -- | 7.5Kva | 7.5Kva | 9 Kva |
9 Kva |
| Power Factor | -- | -- | 0.8 | 0.73 | .08 | .08 |
| Efficiency | -- | 85% | 0.80 | 85% |
85% | |
| Voltage Adjusting Range | -- | -- | 14-26v | 15.5-24v | 14-28v | 16-28v |
| Current Output Range | 50-100 Amps | 20-140A | 40-200A | 30-200A | 40-250A | 40-300A |
| MIG Min./Max. Output (Amps) |
10%@100amps | 30-140Amps: 20% Duty Cycle at 140 Amps |
200amp duty cycle is 40% 155amp duty cycle is 60% 120amp duty cycle is 100% | 200amp duty cycle is 60% | 250amp duty cycle is 35% 200amp duty cycle is 60% 160amp duty cycle is 100% |
40-300Amps 35% Duty Cycle at 300 Amps |
| Wire Speed | -- | 59 to 393 in/min (1.5-10.0m/min) |
59 to 393 in/min (1.5-10.0m/min) | 59 to 393 in/min (1.5-10.0m/min) | 59 to 393 in/min (1.5-10.0m/min) | 59 to 393 in/min (1.5-10.0m/min) |
| Maximum Spool Size Capacity | -- | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder | 30 lb. Internal Spool Feeder |
| Suitable Wire | Welding wire size:.035" to 040" | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. | .8, 1.0 solid/flux cored wire. |
| Spool Gun Capable | NO | SPOOL GUN 140 | Speed Adjust 8M Spool Gun | SPOOL GUN 140 | Speed Adjust 8M Spool Gun | Speed Adjust 8M Spool Gun |
| Weld Aluminum | NO | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN |
YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN | YES, FLUX CORED WIRE OR WITH OPTIONAL SPOOL GUN |
| GMAW-P (Pulse MIG feature ) | NO | No | Yes | No | Yes | Yes |
| Stick Welder (Option) | NO | -- | 40-160Amps 60% Duty Cycle at 160Amps | 30-200Amps 60% Duty Cycle at 160Amps | N/A | N/A |
| DC Stick Material Thickness | -- | -- |
.012- 1/2" | .012- 1/2" | -- | -- |
| Stick ( ARC ) Electrode Maximum Diameter (E7018) | -- | -- | 5/32" | 1/8" | 3/16" | 1/4" |
| Weldable Materials |
Mild Steel | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun | Stainless Steel, Mild Steel, Aluminum with Spool Gun |
30-140Amps:
20% Duty Cycle at 140 Amps
20% Duty Cycle at 140 Amps
- Main Unit with 10ft MIG Torch
- Ground Clamp /li>
- Contact tips
- Stick Electrode Holder
Accessories for this item
Related Articles
Related Videos
Product Literature
Additional resources
Welding Resources
- Preferable MIG welder Review by Sean
-
I use this powerful 2 in 1 welder for general purposes. However, I prefer MIG welding with the gas due to better results in welding bits of thin stainless steel. This machine and a lot of included extras made me glad.
(Posted on Apr 28,2013)
- Affordable and powerful machine Review by Kevin
-
Acquiring this welder provided me with capabilities of doing aluminum using the spool gun that exactly suits my needs in a workshop. It is easily setup in minutes. Thermal overload protection is important for safe and reliable operation. Besides, when buying I got extras - wire roll, welding mask, chipping hammer and welding brush. (Posted on Apr 25,2013)
- good product choice Review by romeroH
-
Trusted product (with all customer service support on this site), 220V, capable of stick and aluminum welding (with additional spool gun), great choice product. Probably needs flux cored wire for the best welding performance. Has a 5 years warranty which is also nice. (Posted on Apr 14,2013)