PROMTS 200i3-in-1 MIG, MIG, TIG and Stick Welder

PROMTS 200i

More Views

MODEL : PROMTS 200i     PRODUCT # : 880161

product Highlights:

3-in-1- 200 Amp MIG, TIG and Stick Welder

Availability: In stock

Retail Price: $1,175.99

Sale Price: $949.99

You will earn 47 Points for buying this product

DOwnload PDF:

Upload images for this product

Have a Question about this Product?
1 Question | 0 Answer
Read all Q&A | Ask a Question
Answer a Question

Recommended Areas Of Use

  • Welding Repair
  • Motorsports/ Automotive
  • Contstruction/HVAC
  • Commercial maintenance
  • Fabrication/machine shops
  • Shipyard/pipeline industry

What’s included

  • 15 AK MIG Gun
  • Ground Clamp
  • 200 Amp Stinger
  • Gas Hose
  • 110/220V Adapter
  • CO2 Regulator
  • 2x Contact Tips
Compare Products

You have no items to compare.

View Additional Photos


Portable MIG-TIG-STICK Unit

The LONGEVITY PROMTS® 200i combines 3 welding processes in 1 machine with an impressive 200 amp MIG welder, 200 amp TIG welder, and 170 amp STICK welder.

Easy Push-Button Setup

The PROMTS® 200i is very user friendly! All the
adjustments are properly spaced and coded which allows
for easy on-the-fly adjustments. The grouped and coded
system allows the user to see the settings quickly and
make necessary adjustments easily, allowing the welder
to more efficient in the workspace and a fine shaped arc!

Powerful, Reliable, Efficient IGBT Technology

Longevity offers cutting-edge technology in the
PROMTS® 200i by including IGBT semiconductors inside
this unit. IGBT technology makes this unit more reliable
than other comparable units using old-fashioned
technology. By using IGBT components, LONGEVITY is
able to offer a potent welder that is lighter and more
space-efficient than its outdated counterparts.

Digital Amp and Volt Meter

By using digital meters, LONGEVITY gives the operator
instantaneous outputs which are easily read while welding.
This allows the user to dial-in their favorite settings
accurately, again, and again!

Larger Wire Spool Capacity

LONGEVITY understands the importance of time and
money. With this PROMPS® 200i, you are able to use 11lb spools for longer welding times without having to
change the spool. This also saves you money as you are
able to buy larger spools at greater discounts. Do not
need to use that much wire? No worries. You are able to
use small 1lb rolls of wire without additional equipment!

Burn Back Control

LONGEVITY uses Burn Back Control to prevent excess
amounts of wire from sticking out by providing extra arc
time without feeding. This allows the user to make
excellent re-starts as smooth and painless as possible.

Stick With Adjustable Arc Force

With Arc Force, you are able to adjust the inductance of
the arc for either a crisp arc or soft arc with a fluid puddle.
This will allow for greater control of your welding
parameters.

Input

110/220 50/60hz 1 phase

Processes

MIG, DC TIG, Stick, Flux Core

Amp Output

MIG: 200amps

TIG: 200amps

Stick: 200amps

Spool Gun Capable

YES

Technology

IGBT Inverter Based

Duty Cycle

MIG: 30% @ 200A

TIG: 35% @ 200A

STICK: 25% @ 200A

Dimensions

W: 10” x H: 15” x D:9”

 

 

 

 

Product Literature :
View FileProMTS 200i Specification Sheet 392.13 KB
View FilePROMTS 200i 1.15 MB
 
Warranty

   

Three year Warranty, parts and labor. Please take a look at our terms and policy page for detailed warranty information on this unit.

 

 LONGEVITY WELDING

WELDMAX 185

WELDMAX® 185i

PROMTS® 252i

INNOVATOR 255I

INNOVATOR® 255i

PROMTS 200i

PROMTS® 200i

Inverter Type Infineon IGBT Infineon IGBT Infineon IGBT Infineon IGBT
Voltage/ Plasma Cutting (PAC) Specs 95% Duty Cycle @ 40 A (220/240) N/A 100% Duty Cycle @ 40 A (220/240) N/A
Recommended Maximum Cut Thickness 3/4" -- 3/4" --
Maximum Severance Cut 1" -- 1" --
Aluminum 3/8" -- 3/8" --
Weld Aluminum No Yes with Optional SpoolGun Yes with Optional SpoolGun Yes with Optional SpoolGun
GTAW-P No Yes Yes No
TIG Welder Specs 10-180Amp at 40% DUTY CYCLE (DC Only) 5-200AMP at 60% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum 10-250AMP at 35% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum MIG/MAG: 30% @ 200A,
STICK/ ARC (SMAW) Welder Specs 10-180AMP at 30% DUTY CYCLE (DC Only) 160AMP at 60% DUTY CYCLE (DC Only) 200AMP at 60% DUTY CYCLE (DC Only) STICK: 25% @ 200A

 

 

200 AMP 3 in 1 AC/DC MIG/TIG/STICK WELDER 110v/220v SpeedAdjust 8m Spool Gun Capable

•   15 AK MIG Gun
•   Ground Clamp
•   200 Amp Stinger
•   CO2 Regulator
•   110v/220v Power Plug adapter
•   2x Contact Tips
•   Gas Hose

Accessories for this item

  1. product Highlights:

    (10 Lanthanated Tungsten Pieces)...
    Sale Price: $105.55
  2. product Highlights:

    Spool gun for the PROMTS 200...

    Retail Price: $412.48

    Sale Price: $329.99

  3. product Highlights:

    Auto Darkening Welding Helmet Adjustable Mask...

    Retail Price: $167.99

    Sale Price: $129.99

Related Articles
Related Videos

Product Literature
Additional resources
Welding Resources

   

Three year Warranty, parts and labor. Please take a look at our terms and policy page for detailed warranty information on this unit.

Be the first to write a review

Questions and Answers
There are no entries.