Follow us on:
Longevity-inc | Twitter Account   Longevity-inc | Face Book Account   Longevity-inc | Face Book Account
Home Login Cart
Click to WIN A FREE LONGEVITY WeldAll 200PI Multi-Process Welding Machine!
  
               
     
   
  Unsubscribe  
     
 
 
Longevity-inc blog | Plasma Cutters and Welders
 
McAfee Secure sites help keep you safe from identity theft, credit card fraud, spyware, spam, viruses and online scams  
   
   
  Switch Off Flash
     
  Products  
  Home » Products » Multi-Purpose Units » WeldAll LS-160P  Bookmark and Share  
 

WeldAll LS-160P/Multi-Purpose Units

 
 
 
 
Click to enlarge
WeldAll LS-160P/Multi-Purpose Units
WeldAll LS-160P/Multi-Purpose Units
WeldAll LS-160P/Multi-Purpose Units
WeldAll LS-160P/Multi-Purpose Units
WeldAll LS-160P
Model: WeldAll LS-160P
Category: Multi-Purpose Units
Purpose:
Details:  
Retail Price: $1,099.99
Sale Price:
$999.99 Qty:    Out Of Stock
Customer Ratings:
Rate This Item
Read Reviews
 
 
 
 
General   Technology   Specifications   What's Included Recommended Accessories   Videos   Warranty
Purpose:
 

WeldAll™ Series Plasma Cutter (AC/DC), Arc welder (AC/DC) and TIG Welder (AC/DC) with Pulse! This unit will weld and cut Aluminum! Unit features Pilot Arc starting technology as seen in Miller and Lincoln plasma cutters. This unit will weld Aluminum! This Multi-Purpose welding machine is completely adjustable in every function! There is nothing left out on this metal cutting and welding multipurpose LONGEVITY machine. This plasma cutter can Cut Aluminum in AC mode, giving you much cleaner and Thicker aluminum cuts than any DC only inverter plasma cutter on the market! This welding machine will run off a normal house 220 outlet (single phase welder and single phase plasma cutter). There is no other company that can compare there welding equipments performance and quality for the price and the satisfaction guarantee that we offer. This machine can weld every kind of metal including copper and stainless steel! not only will it weld any kind of material, but it will also plasma cut any kind of metal as well. You can count on this machine to serve you as an all around metal working machine for years to come. You will not only receive all of your torch and welding leads with this package deal, but you will also receive a foot pedal and an argon regulator! This multipurpose machine along with the rest of our welders and plasma cutters comes with a 5 Year Parts and Labor Warranty + a 30 Day Satisfaction Guarantee!


 
 
 
     
 
Summary   Features   Typical Applications   Manuals
Multi-Purpose Welders Voltage/Plasma Cutting (PAC) Specs
"Rated" Cutting Thicknesses* at 220 V Input  (110V reduces power in half)
Mild Steel Stainless Steel  Aluminum
TIG (GTAW) Welder Specs STICK /ARC (SMAW) Welder Specs Recommended Generator Power

 

WeldMax 416D®   d   40 AMP at 60% DUTY CYCLE (230 V Input)

30 AMP at 60% DUTY CYCLE (110 V Input)
1/2 in 1/2 in 1/4 in 5-160AMP at 60% DUTY CYCLE (DC Only) This will not weld Aluminum 140AMP at 60% DUTY CYCLE (DC Only) 6500 watts
WeldMax 518D®   d   50 AMP at 60% or 40 A at 100% (230 V Input)

40 AMP at 60% or 25 AMP at 100% (110 V Input)
5/8 in 5/8 in 3/8 in 5-180AMP at 60% DUTY CYCLE (DC ONLY) This will not weld Aluminum 160AMP at 60% DUTY CYCLE (DC Only) 7500 watts
WeldMax 520D®   d   50 AMP at 60% or 40 AMP at 100% (230 V Input)

40 AMP at 60% or 30 AMP at 100% (110 V Input)
5/8 in 5/8 in 3/8 in 5-200AMP at 60% DUTY CYCLE (DC ONLY) This will not weld Aluminum 160AMP at 60% DUTY CYCLE (DC Only) 7500 watts
WeldAll 160P®   d   40 AMP at 60% or 30 AMP at 100% (230 V Input) 1/2 in 1/2 in 1/4 in 5-160AMP at 60% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum 140AMP at 60% DUTY CYCLE (DC Only) 10000 watts
WeldAll 200P®   d   50 AMP at 60% or 40 AMP at 100% (230 V Input) 5/8 in 5/8 in 3/8 in 5-200AMP at 60% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum 160AMP at 60% DUTY CYCLE (DC Only) 12000 watts
WeldAll 160PI®   d d 70 AMP at 60% (230 V Input) 5/8 in 5/8 in 3/8 in 5-160AMP at 60% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum 160AMP at 60% DUTY CYCLE (DC Only)

 

12000 watts
WeldAll 200PI®   d d 50 AMP at 60% or 40 AMP at 100% (230 V Input) 3/4 in 3/4 in 1/2 in

5-200AMP at 60% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum

180AMP at 60% DUTY CYCLE (DC Only) 12000 watts
WeldAll 250PI®   d d 50 AMP at 60% or 40 AMP at 100% (230 V Input) 1 in 1 in 5/8 in  5-250AMP at 60% DUTY CYCLE (AC/DC GTAW PULSE) This will weld Aluminum 190AMP at 60% DUTY CYCLE (DC Only) 15000 watts
 
     
 
Class Key:        
d Hobbyist d Light Industrial d Industrial
 
     
 
Quality Key:        
d Designed for this process d Capable of this process    
 
     
     
 
  View All Multi-Purpose Units
 
     
 
  Multi-Purpose Units
Resources
 
 
     
 
  If you have any questions about this product, please fill out this contact request form or chat live with one of our sales representatives.  
           
Country:   Phone#:   *
Company (optional):   Fax:  
Your Name:   * Email:   *
Address:   * Retype E-mail Address:   *
City:   *      
State:   *      
Zip/Postal Code:   *      
 
Subscribe me to Longevity™ newsletters:   Subscribe to Newsletters
Where did you hear about us?  
Your question:  
   
Try a new code
Type the Word   *Please enter the security code in all capitalized (UPPER CASE) letters
Please allow 24-48 hours for a response. For immediate assistance, please try our live chat or call our toll free number at 1-877.LONG.INC / 1.877.566.4462.
   
 
 
     
   
     
   
 
Longevity Hot Welding Products
 
Home | About Us | Products | Rentals | Resources | Welding Forum | Dealers | Order Status | Contact Us | Help & FAQs | Site Map | Terms and Policy | Useful Links | Welders Plasma Cutters Specials | Video Library | Manuals & Forms | About Us | Company Info | News | Shows | History | Product Registration | Customer of the month| Blog
© 2009 longevity-inc.com Longevity Global, Inc. 23591 Foley St, Hayward CA 94545

SSL Certificates