CERIATED 2% GREY 1/16" (1.6mm)

Sale Price $6.99 Regular Price $7.99
In stock
SKU
741360253926
LEASE IT
For Businesses

The Longevity CERIATED 2% GREY electrodes are recommended for short welding cycles on low-amp, DC orbital tube, pipe, thin sheet, and small part applications. Provides low current and arc ignition with good arc stability.