Portable MIG-TIG-STICK Unit

The LONGEVITY MULTIMIG® 252 MP combines 3 welding processes in 1 machine with an impressive 250 amp MIG welder, 250 amp TIG welder, and 250 amp STICK welder.

Easy Push-Button Setup

The MULTIMIG® 252 MP is very user friendly! All the
adjustments are properly spaced and coded which allows
for easy on-the-fly adjustments. The grouped and coded
system allows the user to see the settings quickly and
make necessary adjustments easily, allowing the welder
to more efficient in the workspace and a fine shaped arc!

Powerful, Reliable, Efficient IGBT Technology

Longevity offers cutting-edge technology in the
MULTIMIG® 252 MO by including IGBT semiconductors inside
this unit. IGBT technology makes this unit more reliable
than other comparable units using old-fashioned
technology. By using IGBT components, LONGEVITY is
able to offer a potent welder that is lighter and more
space-efficient than its outdated counterparts.

Digital Amp and Volt Meter

By using digital meters, LONGEVITY gives the operator
instantaneous outputs which are easily read while welding.
This allows the user to dial-in their favorite settings
accurately, again, and again!

Larger Wire Spool Capacity

LONGEVITY understands the importance of time and
money. With this MULTIMIG® 252 MP, you are able to use 11lb spools for longer welding times without having to
change the spool. This also saves you money as you are
able to buy larger spools at greater discounts. Do not
need to use that much wire? No worries. You are able to
use small 1lb rolls of wire without additional equipment!

Burn Back Control

LONGEVITY uses Burn Back Control to prevent excess
amounts of wire from sticking out by providing extra arc
time without feeding. This allows the user to make
excellent re-starts as smooth and painless as possible.

Stick With Adjustable Arc Force

With Arc Force, you are able to adjust the inductance of
the arc for either a crisp arc or soft arc with a fluid puddle.
This will allow for greater control of your welding
parameters.

Input

90v-270v 50/60hz 1 phase

Spool Gun Capable

YES with the Speedadjust 8m SpoolGun

Technology

IGBT Inverter Based

Duty Cycle

MIG

60% @ 150A

60% @ 250A

STICK

60% @ 110A

60% @ 250A

TIG

60% @ 150A

60% @ 250A

Stick Welding Capable

YES

Tig Welding Capable 

YES

Dimensions

W: 9.5” x H: 18” x D: 25”

Weight

56 lbs

 

 

 

  • 24KD MIG Gun
  • Ground Clamp
  • 200 Amp Stinger
  • Gas Hose
  • 110/220V Adapter
  • CO2 Regulator
  • MIG Consumables
  • Tig
  • Mig
  • Stick
  • Multiprocess
  • Plasma
  • CNC
  • Consumables
  • Welding Armor
  • General
  • Setup
<ul>
<li>Welding Repair</li>
<li>Motorsports/ Automotive</li>
<li> Contstruction/HVAC</li>
<li> Commercial maintenance</li>
<li> Fabrication/machine shops</li>
<li> Shipyard/pipeline industry</li>
</ul>

   

One year Warranty, parts and labor. Please take a look at our terms and policy page for detailed warranty information on this unit.