 Filler Rods are essential to TIG (GTAW) Welding because the filler rod is fed into the molten puddle by hand filling in the puddle to create a stronger metal bond or puddle to join two metal pieces. It is extremely important to have the right filler rod based on the metal you are welding whether it is mild steel, aluminum, stainless steel, copper, bronze, and other exotic metals. It is also necessary to have the right tungsten to insure you are properly setup to weld your metal. Our Plasma Cutters, Stick Welding Equipments, TIG Welders, MIG Welders are under the industry leading warranty!*

LONGEVITY WELDING PRODUCT NAME TYPE AWS DIAMETER inches (mm) LENGTH inches(mm) SHIELDING GAS FEATURES TYPICAL USES
THUNDER ROD 4043 1/16 THUNDER ROD 4043 1/16"(1.6mm) aluminum ER4043 1/16"(1.6) 36"(914.4) 100% aluminum and many weldable cast aluminum alloys bicycle frames pressure vessels
THUNDER ROD ER4043 3/32 THUNDER ROD ER4043 3/32"(2.4mm) aluminum ER4043 3/32"(2.4) 36"(914.4) 100% aluminum and many weldable cast aluminum alloys bicycle frames pressure vessels
THUNDER ROD ER4043 1/8 THUNDER ROD ER4043 1/8"(3.2mm) aluminum ER4043 1/8"(3.2) 36"(914.4) 100% aluminum and many weldable cast aluminum alloys bicycle frames pressure vessels
THUNDER ROD ER5356 1/16 THUNDER ROD ER5356 1/16"(1.6mm) aluminum ER5356 1/16"(1.6) 36"(914.4) 100% aluminum magnisium , for many weldable cast aluminum alloys architectural structures and vehicles
THUNDER ROD ER5356 3/32"(2.4mm) THUNDER ROD ER5356 3/32"(2.4mm) aluminum ER5356 3/32"(2.4) 36"(914.4) 100% aluminum magnisium , for many weldable cast aluminum alloys architectural structures and vehicles
THUNDER ROD ER5356 1/8 THUNDER ROD ER5356 1/8"(2.4mm) aluminum ER5356 1/8"(3.2)  36"(914.4) 100% aluminum magnisium , for many weldable cast aluminum alloys architectural structures and vehicles
LONGEVITY WELDING PRODUCT NAME PRODUCT # TYPE AWS DIAMETER inches (mm) LENGTH inches(mm) SHIELDING GAS FEATURES TYPICAL USES
LONGEVITY WELDING THUNDER ROD ER70S-6 1/16"(1.6mm) 880348 mild steel ER70S-2 1/16"(1.6) 18"(457.2) 100% multiple deoxidized, high quality welds in many carbon steels great for pipe welding, sheet metal applications root pass pipewelding applications
THUNDER ROD ER70S-2 3/32
THUNDER ROD ER70S-6 3/32"(2.4mm)
880350 mild steel ER70S-2 3/32"(2.4) 18"(457.2) 100% multiple deoxidized, high quality welds in many carbon steels  great for pipe welding, sheet metal applications root pass pipewelding applications
THUNDER ROD ER70S-2 1/8 THUNDER ROD ER70S-6 1/8"(3.2mm) 880352 mild steel ER70S-2 1/8"(3.2) 18"(457.2) 100% multiple deoxidized, high quality welds in many carbon steels great for pipe welding, sheet metal applications root pass pipewelding applications

Pick the Right Filler Rod for Steel or Aluminum

LONGEVITY Company provides filler rods of high quality and at reasonable prices. Please check the selection of filler rods that we provide and decide which is the best rod application that you should use for your weld. Choosing the right filler rod is very important for the matter density and the strength of your weld. Pick the right rod by determining the diameter of the filler rod that is needed, by checking the thickness of the material that will be weld. Here are some pointers in deciding how to choose the correct filler rod for your weld.

 

Check these 6 Points when selecting Filler Rods:

1. 4043 is a general filler rod, usually used for aluminum welding.
2. 5356 is perfect for 5xxx series aluminum. If you are planning on anodizing the finished piece, this rod should be used when making the weld.
3. ER70S-6 is used for welding mild steel.
4. ER70S-2 is recommended for welding 4130 chrome moly tubing in many applications.
5. ER80S-D2 is for welding 4130 chrome moly tubing in case a higher strength weld is needed.
6. 1/16” diameter filler rod to be used when material is 1/8” and less thick. 3/32” diameter filler rod should be used for 1/8” and thicker material.