Excellent Versatility and Plasticity
The Longevity ALLOY-ARC ER5356 has great corrosion resistance against exposure to salt water along with high strength. The 5356 is typically chosen to weld 2XXX, 3XXX and 6XXX series base metals.
The Longevity ALLOY-ARC ER5356 has great corrosion resistance against exposure to salt water along with high strength. The 5356 is typically chosen to weld 2XXX, 3XXX and 6XXX series base metals. Another great feature is its resistance to cracking and the fact that it promotes penetration better than other filler metals.
Advantages:
• General purpose MIG filler metal because of its excellent weldability and plasticity
• Resists cracking and produces quality welds almost smut free
• A popular choice due to its versatility
• Leaves your finished weld looking bright and shiny
| Specifications | 0.035"(0.9mm), 1Lb Spool |
|---|---|
| What's Included | 1 wire spool |
| Inverter Type | ER5356 |
| Typical Use | Aluminum |
| Product # | 880492 |
| Contact Tip Size | 0.035" (0.9 mm) |
| Weight lb / kg | 1lb / .5kg |
This product can expose you to chemicals including Formaldehyde (gas), which is known to the State of California to cause cancer. For more information go to www.p65warnings.ca.gov
-
-
-
-
- MIG WELDING GLOVES, WELDING-ARMOR M04 (Large) Reinforced Leather, Extreme Comfort, Maximum Protection$19.99
-








