The Longevity CERIATED TUNGSTEN 2% GRAY electrodes are recommended for short welding cycles on low-amp, DC orbital tube, pipe, thin sheet, and small part applications. Provides low current and arc ignition with good arc stability.
TIG Tungsten Electrodes & Diameters - 2% Thoriated, Lanthanated, Ceriated
Introduction
2% Ceriated is an excellent substitute for 2% Thoriated tungsten and is designed for transformer and inverter based power sources. For transformer DC welding, this tungsten requires less amperage to start, so it is recommended for thinner metals.
Depending on the additives, desired results can include a stable arc in both AC and DC processes, greater longevity than thoriated tungsten, the ability to use a smaller-diameter electrode for the same job, use of a higher current for a similar-sized electrode, and less tungsten spitting.
Benefits:
• Requires less amperage to start
• Easy arc starting
• Good arc stability
• Long life
• High current capacity
• Possible replacement for thoriated
| Product Features | Size: 1/8" x 7" or 3.2mm x 175mm |
|---|---|
| Specifications | 1/8"(3.2mm), 10-Pack |
| What's Included | 10 electrodes |
| Typical Use | Aluminum, Magnesium, Nickel, Copper, Titanium, Low-alloyed Steels |
| Product # | 880098 |
This product can expose you to chemicals including Formaldehyde (gas), which is known to the State of California to cause cancer. For more information go to www.p65warnings.ca.gov
-
-
-
- TIG / PLASMA CUTTING GLOVES, WELDING-ARMOR T02 (X-Large) Reinforced Leather, Extreme Comfort, Maximum Protection$19.99
- TIG / PLASMA CUTTING GLOVES, WELDING-ARMOR T01 (X-Large) Reinforced Leather, Extreme Comfort, Maximum Protection$19.99
-