Premium AWS Class MIG Welding Wire
Longevity ER70S-6 0.023" Carbon Steel MIG welding wire comes on an 11 lb spool and contains deoxidizers that offer better wetting, providing a flatter bead shape and faster travel speeds. This general-purpose wire is used with 100% carbon dioxide, 75/25 shielding gas or with higher contents of argon like 90/10 for fabrication of mild steel. Wire conforms to AWS A5.18 ER70S-6.
Longevity ER70S-6 0.023" Carbon Steel MIG welding wire comes on an 11 lb spool and contains deoxidizers that offer better wetting, providing a flatter bead shape and faster travel speeds. This general-purpose wire is used with 100% carbon dioxide, 75/25 shielding gas or with higher contents of argon like 90/10 for fabrication of mild steel. Wire conforms to AWS A5.18 ER70S-6.
Features:
• Premium AWS CLASS ER70S-6Â
• For general purpose MIG WeldingÂ
• Designed to be used on mild steelÂ
• Best used with clean or prepared welding surfaceÂ
• Requires a shielding gasÂ
• DC reverse polarityÂ
• Spool Size: 11 lbsÂ
• Wire Size: 0.023"
| Specifications | 0.023"(0.6mm), 11Lb Spool |
|---|---|
| What's Included | 1 wire spool |
| Inverter Type | ER70S-6 |
| Typical Use | Carbon Steel |
| Product # | 880480 |
| Contact Tip Size | 0.023" (0.6 mm) |
| Weight lb / kg | 11lb / 5kg |